주철관의 잔존강도 평가에 관한 연구

sessment of residual tensile strength on cast iron water pipes

초록

The goal of this study is to assess cast iron pipes(CIPs) and present a residual tensile strength prediction model using pit characteristics and fracture toughness. The results is the followings. First, average pit depths of collected CIPs were in the range from 0.63 to 6.49 mm, loss of tensile strength compared with net metallic tensile strength were from -7.06 to 67.91 percent. Second, fracture toughness for NS-CR-1, NS-CR-2, and NS(2)-CR-1 were in the range from 62.85 to 89.39 kgf/㎟ , and average of those samples was 73.69 kgf/㎟ on CIPs. Third, the models developed in this study by using pit characteristics and fracture toughness showed a little good correlation for measured residual tensile strength, and the results will be expected to help for water utilities to manage CIPs in the aspect of rehabilitation and assessment of structural safety on CIPs

키워드

Water pipe; Pit corrosion; Residual strength; Fracture toughness; 상수도관; 공식; 잔존강도; 파괴인성* Corresponding author Tel:+82-42-860-0387; Tel:+82-42-860-0399; Email : juhwan@kowaco.or.kr(Kim; J.H); Water pipe; Pit corrosion; Residual strength; Fracture toughness
제목
주철관의 잔존강도 평가에 관한 연구
제목 (타언어)
sessment of residual tensile strength on cast iron water pipes
저자
배철호; 홍성호; 김주환; 김정현
발행일
2006-12
저널명
상하수도학회지
권
20
호
6
페이지
867 ~ 874