In this study, the residual strength prediction models were proposed by measuring various residual strength according to pit characteristics for metallic water pipes such as cast iron pipe (CIP), ductile iron pipe (DIP), and steel pipe (SP). The exponential prediction model was better fitted to measured residual tensile strength for CIP. In case of DIP and SP, the prediction model using loss of strength was more exactly predicted compared with other model types. The fracture toughness were averagely 40.46 for CIP, 85.27 for DIP, and 97.27 for SP, the determination coefficient () of between measured residual tensile strength and predicted values for residual strength prediction models using fracture toughness was estimated from 0.44 to 0.86. Especially, the proposed residual tensile strength prediction models were applied for the verification and reliability to CIPs and DIPs at 14 sites. The determination coefficient () between measured residual tensile strength and predicted values was estimated from 0.76 to 0.78. Therefore it was thought that the proposed residual tensile strength models could help to support resonable and economical decision of rehabilitation/replacement.
키워드
- 제목
- 상수도 금속관의 잔존 인장강도 추정모델 개발
- 저자
- 배철호; 김정현; 우형민; 홍성호
- 발행일
- 2008
- 저널명
- 한국지반환경공학회 논문집
- 권
- 9
- 호
- 3
- 페이지
- 17 ~ 28
- 출판사
- 한국지반환경공학회
- 발행국가
- 대한민국
- 분량
- 12 페이지
- ISSN
- P 1598-0820